Sign In | Join Free | My burrillandco.com
Home > Return Bend >

U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater

    Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers
     
    Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers
    • Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers
    • Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers
    • Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers
    • Buy cheap U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater from wholesalers

    U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater

    Ask Lasest Price
    Brand Name : Yuhong
    Model Number : 180 DEG. ELBOW
    Certification : ABS, BV, DNV, CCS, LR
    Price : Negotiable
    Payment Terms : TT, LC
    Supply Ability : 10000 Tons/Month
    Delivery Time : 5 - 90 Days
    • Product Details
    • Company Profile

    U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater

    U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater


    Alloy C22 is a nickel-chromium-molybdenum solid solution reinforced superalloy with a nominal chemical composition of 56% nickel, 22% chromium and 13% molybdenum with additions of iron, tungsten and cobalt. It is commonly known as Hastelloy C22 and generic name UNS NO6022.


    Hastelloy C22 is a general purpose nickel-chromium-molybdenum-tungsten austenitic alloy with increased resistance to pitting, crevice corrosion and stress corrosion cracking. The high chromium content gives good oxidation resistance to oxidizing media, while the molybdenum and tungsten content gives good oxidation resistance to reducing media.

    Hastelloy C22 also has excellent resistance to oxidizing aqueous media, including wet chlorine and mixtures containing nitric acid or oxidizing acids with chloride ions.

    Hastelloy C22 should not be used at service temperatures above 1250°F due to formation of harmful phases above this temperature.


    Chemical Composition

    Grade

    C

    Mn

    Si

    Cu

    S

    Fe

    Ni

    Cr

    P

    Mo

    Hastelloy C22

    0.010 max

    0.50 max

    0.08 max

    0.50 max

    0.02

    2.00 – 6.00

    50.015 min

    20.00 – 22.50

    0.02 max

    12.50 – 14.50


    Equivalent Grades

    STANDARD

    WERKSTOFF NR.

    UNS

    JIS

    GOST

    EN

    Hastelloy C22

    2.4602

    N06022

    NW 6022

    NiCr21Mo14W


    Mechanical & Physical Properties

    Density

    8.69 g/cm3

    Melting Point

    1399 °C (2550 °F)

    Tensile Strength

    Psi – 1,00,000 , MPa – 690

    Yield Strength (0.2%Offset)

    Psi – 45000 , MPa – 310

    Elongation

    45 %


    Applications:

    • 1. Chemical processing
    • 2. Pharmaceutical industry
    • 3. Petrochemical industry
    • 4. Waste treatment facilities
    • 5. Power generation
    • 6. Pulp and paper industry
    • 7. Food processing industry

    U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater


    Quality U Bend Return , ASTM B366 C22 , NO6022 Hastelloy 180Deg. Elbow SR , Fired Heater for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: YUHONG HOLDING GROUP CO., LTD
    *Subject:
    *Message:
    Characters Remaining: (0/3000)